Irradiation cross-linked low-smoke halogen-free flame-retardant sheath material is made of high-purity resin as the base material, with halogen-free flame retardant, cross-linking agent, antioxidant, etc. mixed and extruded into granules. It has excellent properties such as halogen-free, heat-resistant, flame-retardant, low-smoke, and weather-resistant. It has no precipitation pollution, meets the relevant requirements of Rohs, and is easy to extrude and process.
Application: wire and cable for construction.
| Test items | Value | Typical Value | Unit | Method |
| Physical property | ||||
| Hardness | 92±3 | 92 | Shore A | GB/T 2411 |
| Density | ≤1.68 | 1.65 | g/cm3 | GB-T 1033 |
| Low temperature embrittlement temperature | ≤15/30 | 0/30 | PCS | GB/T 5470 |
| Tensile strength before irradiation | ≥8 | 8.8 | MPa | GB/T 1040 |
| Elongation at break before irradiation | ≥160 | 168 | % | GB/T 1040 |
| Tensile strength before aging | ≥10 | 12.2 | MPa | GB/T 1040 |
| Elongation at break before aging | ≥125 | 150 | % | GB/T 1040 |
| Thermal elongation 0.2MPa×200℃×15min | ||||
| Elongation under load | ≤100 | 40 | % | GB/T 2951 |
| Permanent deformation | ≤25 | 0 | % | GB/T 2951 |
| Aging performance 135℃×168h | ||||
| Tensile strength change rate | ≤-30 | -18 | % | GB/T2951.12 |
| Change rate of elongation at break | ≤-30 | -20 | % | GB/T2951.12 |
| Electrical performance | ||||
| 20℃ volume resistivity | ≥1.0×1014 | 2.7×1014 | Ω.cm | GB/T 1410 |
| Dielectric strength | ≥20 | 22 | MV/m | DIN EN 6024 |
| Flame retardant and combustion performance | ||||
| Oxygen index | ≥30 | 36 | % | GB/T 2406 |
| Halogen acid gas generation | ≤0.5 | 0.1 | mg/g | IEC 60754 |
| PH value | ≥4.3 | 5.5 | - | IEC 60754 |
| Electrical conductivity | ≤2.5 | 2 | μs/mm | IEC 60754 |
| Smoke density (with flame) | ≤100 | 85 | - | GB/T 8323 |
| Peak heat release rate | ≤180 | 150 | kW/m2 | ISO/5660 |
| Total heat release | ≤180 | 105 | MJ/m2 | ISO/5660 |
| Average heat release rate | ≤100 | 74 | kW/m2 | ISO/5660 |